Effect of Fluoride Mouthrinses on Flexural Strength and Microhardness of 3D Printed CAD Temporary Provisional Resins

Document Type : Original Article

Authors

1 Department of Prosthodontics, School of Dentistry, Dental implant research center, Hamadan University of Medical Sciences, Hamadan, Iran

2 Department of Prosthodontics, School of Dentistry, Dental implant research center, Hamadan University of Medical Sciences, Hamadan, Iran.

3 Resident in Dental Prosthetics, School of Dentistry, Hamadan University of Medical Sciences, Hamadan, Iran

4 Department of Biostatistics, School of Public Health and Research Center for Health Sciences, Hamadan University of Medical Sciences, Hamadan, Iran.

10.30476/dentjods.2026.108864.2846
Abstract
Background: Despite the high accuracy of 3D-printed provisional restorations, their clinical longevity is influenced by resin chemistry and processing. Current evidence is insufficient to determine how these materials, specifically their flexural strength and surface microhardness, respond to daily exposure to fluoride mouthrinses

Purpose: This study evaluates the effect of a fluoride-containing mouthrinse on flexural strength and microhardness of 3D-printed provisional resins.

Materials and Method: In a 2024 in-vitro study, rectangular specimens (25×2×2 mm; n = 96; 48/resin) from two DLP-printed provisional resins (Detax, Arma) were assigned to three media (n = 16/cell): Baseline (no immersion), artificial saliva (AS, 37 °C), and AS with twice-daily 1-minute immersion in alcohol-free fluoride mouthrinse (225 ppm F⁻; FE). Flexural strength was measured by three-point bending; surface hardness by Vickers microhardness (VHN).

Results: Detax showed higher flexural strength than Arma in all media (all p<0.001), with mean differences of 21.9 MPa (Baseline), 24.9 MPa (AS), and 24.4 MPa (FE). For microhardness, Detax exceeded Arma at Baseline (Δ = 0.09 VHN, p = 0.014) and FE (Δ = 0.09 VHN, p<0.001), but not in AS (p = 0.267). Within each resin, one-way ANOVA showed significant medium effects for flexural strength (both p<0.001), with Baseline > AS and Baseline > FE; however, no statistically significant difference was observed between AS and FE. Two-way ANOVA indicated significant main effects of Resin and Medium for both endpoints (all p<0.001), with no significant interaction terms, indicating additive influences.

Conclusion: Brief repeated exposure to artificial saliva and a fluoride mouthrinse demonstrably reduced flexural strength and microhardness of DLP-printed provisionals; DETAX consistently exhibited superior performance compared with ARMA. Comparable flexural losses across media implicate water-driven plasticization/hydrolysis rather than fluoride per se, while fluoride accentuated surface softening only in ARMA. Durability therefore hinges on material selection and counseling toward neutral-pH, alcohol-free rinses.

Keywords



Articles in Press, Accepted Manuscript
Available Online from 18 November 2026

  • Receive Date 29 September 2025
  • Revise Date 23 September 2026
  • Accept Date 17 November 2026
  • First Publish Date 18 November 2026
  • Publish Date 18 November 2026